To a certain the required properties of stones, the following tests can be conducted:
(i) crushing strength test
(ii) water absorption test
(iii) abrasion test
(iv) impact test
(v) acid test.
(I) crushing strength test
For directing this test, an example of size 40 × 40 × 40 mm are set up from parent stone. At that point, the sides are finely dressed and set in water for 3 days. The immersed example is furnished with a layer of plaster of Paris on its top and base surfaces to get even surface so that heap applied is conveyed consistently. Uniform burden dissemination can be acquired sufficiently by giving a couple of 5 mm thick plywood as opposed to utilizing mortar of Paris layer moreover. The example so positioned in the pressure testing machine is stacked at the pace of 14 N/mm2 per minute. The devastating burden is noted. At that point, smashing strength is equivalent to the devastating burden separated by the territory over which the heap is applied. At any rate, three examples should be tried and the normal should be taken as crushing strength.
क्रशिंग स्ट्रेंथ टेस्ट: इस टेस्ट को आयोजित करने के लिए, आकार 40 × 40 × 40 मिमी के नमूने हैं ,मूल पत्थर से तैयार। फिर पक्षों को बारीक कपड़े पहनाए जाते हैं और 3 दिनों के लिए पानी में रखा जाता है। ,संतृप्त नमूने को इसके ऊपर और नीचे की सतहों पर प्लास्टर ऑफ पेरिस की एक परत के साथ प्रदान किया जाता है, सतह ताकि लोड लागू समान रूप से वितरित किया जाता है। वर्दी लोड वितरण प्राप्त किया जा सकता है, प्लास्टर ऑफ पेरिस लेयर का उपयोग करने के बजाय 5 मिमी मोटी प्लेवुड की एक जोड़ी प्रदान करके संतोषजनक रूप से।संपीड़न परीक्षण मशीन में रखा गया नमूना 14 N / mm2 प्रति की दर से भरा हुआ है , मिनट। पेराई भार नोट किया गया है। फिर पेराई ताकत पेराई किए गए पेराई भार के बराबर है वह क्षेत्र जिस पर भार लागू किया जाता है। कम से कम तीन नमूनों का परीक्षण किया जाना चाहिए और औसत होना चाहिए कुचल शक्ति के रूप में लिया।
ii) Water Absorption Test
For this test cube specimen weighing about 50 grams are prepared and the test is carried out in the steps given below:
(a) Note the weight of dry specimen as W1.
(b) Place the specimen in water for 24 hours.
(c) Take out the specimen, wipe out the surface with a piece of cloth and weigh the specimen. Let its weight be W2.
(d) Suspend the specimen freely in water and weigh it. Let its weight be W3.
(e) Place the specimen in boiling water for 5 hours. Then take it out, wipe the surface with cloth and weigh it. Let this weight be W4. Then,
इस परीक्षण के लिए लगभग 50 ग्राम वजन वाले क्यूब नमूने को तैयार किया जाता है और परीक्षण नीचे दिए गए चरणों में किया जाता है:
(ए) शुष्क नमूने के वजन को W1 के रूप में नोट करें।
(b) पानी में नमूना २४ घंटे के लिए रखें।
(c) नमूना बाहर निकालें, सतह को कपड़े के टुकड़े से पोंछें और नमूना बुनें। इसका वजन W2 होने दें।
(d) पानी में स्वतंत्र रूप से नमूने को निलंबित करें और उसका वजन करें। इसका वजन W3 होने दें।
(spec) उबलते पानी में नमूने को ५ घंटे के लिए रखें। फिर इसे बाहर निकालें, सतह को कपड़े से पोंछें और इसे तौलना। इस वजन को W4 होने दें। फिर,
(iii) abrasion test
This test is carried out on stones which are used as aggregates for road construction. The test result indicate the suitability of stones against the grinding action under traffic. Any one of the following test may be conducted to find out the suitability of aggregates:
(i) Los Angeles abrasion test
(ii) Deval abrasion test
(iii) Dorry’s abrasion test.
यह परीक्षण पत्थरों पर किया जाता है जो सड़क निर्माण के लिए समुच्चय के रूप में उपयोग किए जाते हैं। परीक्षा परिणाम यातायात के तहत पीसने की कार्रवाई के खिलाफ पत्थरों की उपयुक्तता का संकेत देता है। समुच्चय की उपयुक्तता का पता लगाने के लिए निम्नलिखित में से कोई एक परीक्षण आयोजित किया जा सकता है:
(i) लॉस एंजिल्स घर्षण परीक्षण
(ii) देवल घर्षण परीक्षण
(iii) डोर्री का घर्षण परीक्षण।
The Los Angeles device [Fig .underneath ] comprises of an empty chamber 0.7 m inside measurement and 0.5 m long with the two finishes shut. It is mounted on an edge so it very well may be pivoted about the level hub. Alongside indicated weight of example, a predefined number of cast iron chunks of 48 mm distance across are put in the chamber. At that point, the chamber is pivoted at a speed of 30 to 33 rpm for a determined number of times (500 to 1000). At that point, the total is taken out and sieved at 1.7 mm. IS strainer. The heaviness of total passing is found.
लॉस एंजेलिस उपकरण [चित्र। बिलो] में एक खोखला सिलेंडर होता है जिसका व्यास ०.० मीटर और व्यास ०.५ मीटर लंबा होता है और दोनों सिरे बंद होते हैं। इसे एक फ्रेम पर लगाया गया है ताकि इसे क्षैतिज अक्ष के बारे में घुमाया जा सके। नमूना के निर्दिष्ट वजन के साथ सिलेंडर में 48 मिमी व्यास के कच्चे लोहे की गेंदों की एक निर्दिष्ट संख्या रखी गई है। फिर सिलेंडर को निर्दिष्ट संख्या (500 से 1000) के लिए 30 से 33 आरपीएम की गति से घुमाया जाता है। फिर कुल को हटा दिया जाता है और 1.7 मिमी पर छलनी किया जाता है। चलनी है। कुल पासिंग का वजन पाया जाता है।
(iv) impact test
\The obstruction of stones to affect is found by leading tests in impact testing machine . It comprises of an edge with guides in which a metal hammer gauging 13.5 to 15 kg can uninhibitedly tumble from a tallness of 380 mm. Totals of size 10 mm to 12.5 mm are filled in chamber in 3 equivalent layers; each layer is packed multiple times. The equivalent is then moved to the cup and again packed multiple times. The hammer is then permitted to fall uninhibitedly on the example multiple times. The example is then sieved through 2.36 mm sieves.
परीक्षण मशीन (अंजीर। नीचे) को प्रभावित करने में परीक्षण करने के लिए पत्थरों का प्रतिरोध पाया जाता है। इसमें गाइड के साथ एक फ्रेम होता है जिसमें 13.5 से 15 किलोग्राम वजन का एक धातु का हथौड़ा स्वतंत्र रूप से 380 मिमी की ऊंचाई से गिर सकता है। 10 मिमी से 12.5 मिमी के आकार के एग्रीगेट 3 समान परतों में सिलेंडर में भरे जाते हैं; प्रत्येक परत को 25 बार टैम्प किया जा रहा है। उसी को फिर कप में स्थानांतरित किया जाता है और फिर से 25 बार टैम्प किया जाता है। फिर हथौड़ा को 15 बार नमूना पर स्वतंत्र रूप से गिरने की अनुमति दी जाती है। नमूना फिर 2.36 मिमी छलनी के माध्यम से छलनी है।
Enable GingerCannot connect to Ginger Check your internet connection
or reload the browserDisable in this text fieldEditEdit in GingerEdit in GingerEnable GingerCannot connect to Ginger Check your internet connection
or reload the browserDisable in this text fieldEditEdit in GingerEdit in GingerEnable GingerCannot connect to Ginger Check your internet connection
or reload the browserDisable in this text fieldEditEdit in GingerEdit in GingerEnable GingerCannot connect to Ginger Check your internet connection
or reload the browserDisable in this text fieldEditEdit in GingerEdit in GingerEnable GingerCannot connect to Ginger Check your internet connection
or reload the browserDisable in this text fieldRephraseRephrase current sentenceEdit in Ginger
No comments:
Post a Comment
if you have any doubt please let me know
Note: Only a member of this blog may post a comment.